420 1.4021 SUS420J1 Stainless Steel Bar

  • group nameStainless Steel Bars

  • Min Order1 piece

  • brand namefushun

  • modelAISI 420

  • payment methodL/C, T/T

  • update timeThu, 14 Oct 2021 14:41:35 GMT

Paramtents

  • Delivery condition annealed

  • Surface condition Black, Machined

  • Similar grades AISI 420 2Cr13 S42020

  • Standard ASTM A276

Packging & Delivery

  • Min Order1 piece

Briefing

AISI 420 1.4021 SUS420J1 S42020 Stainless Steel is a martensitic stainless steel that offers a high hardenability and strength

Detailed

Introduction AISI 420

AISI 420 Stainless Tool Steel is a martensitic stainless steel with 12% Chromium which is sufficient to give good corrosive resistance properties. It’s best corrosive resistance is when hardened and surface is ground or polished.It has good ductility in the annealed condition but can be hardened up to 500HB (highest of the chromium grades). Martensitic Grades are known for high hardness and allowances must be made for poor weldability and usually allowances for a final harden and temper treatment. Steel is magnetic and welding is not recommended.

AISI 420 Applications

Moulds for corrosive plastic materials such as PVC, recycled polymers etc., moulds for chemically aggressive plastics and plastics containing abrasive fillers, mould inserts, dies and gauges for PVC extrusions, screws and barrels for extruders, moulds for automotive, food, medical and optical industry such as spectacles, compact discs, lenses.

Standard

AISI 420 Chemical Composition(%)

C

Si

Mn

P

S

Cr

Ni

Mo

0.15 min

1.0 max

1.0 max

0.040 max

0.030 max

12.0-14.0

0.75 max

0.50 max

Size and Delivery Condition
Diameter : 10-300 mm ; Length Max 9 meters.
Optional Process : Hot rolled / Cold Drawn
Delivery Condition : Annealed 
Surface ; Bright / Ground / Peeled

AISI 420 Mechanical Properties (Q+T)

Tensile Strength (Mpa)

Yield Strength (Mpa)

Elongation (%)

Hardness (HB)

850-1000

600 min

12 min

280 min

AISI 420 Heat Treatment

Annealing: 

For maximum softness, heat uniformly to 1500 – 1650°F (816 – 899°C) and cool slowly in the furnace.


Stress Relieving: 

Heat at 300 – 800°F (149 – 427°C) for 1 to 3 hours, cool in air or quench in oil or water.


Hardening: 

Preheat, then heat to 1800 -1950°F (982 – 1066°C), soak at temperature and air cool or quench in warm oil.

Nearest port for product export
Tianjin, Qingdao, Shanghai, Huangshi
Delivery clauses under the trade mode
FOB, CFR, CIF, CIP, CPT, DDP, DDU, DAF
Acceptable payment methods
T/T, L/C, D/P D/A
Contact Suppliers

Follow this Suppliers