group nameAlloy Steel Bars
Min Order1 piece
brand namefushun
model16MnCr5 1.7131
payment methodT/T, L/C, D/P D/A
update timeTue, 28 Jun 2022 13:47:52 GMT
Delivery Condition normalised and tempered/softened
Min Order1 piece
Grade :16MnCr5
Number:1.7131
Classification: Alloy special steel
Diameter : 80 to 600 mm ;
Length : 1000 to 9000 mm ;
Our advantage :
1. High Quality, Reasonable Price
2. Over 40 Years Experience
3. ISO NQA Certificated Factory
4. Worldwide shipping
5. Emergency Orders and Fast Delivery
Equivalent grades of steel 16MnCr5 (1.7131)
EU | USA | Germany | France | England | Italy |
EN | - | DIN,WNr | AFNOR | BS | UNI |
16MnCr5 | SAE5115 | 16MnCr5 | 16MC5 | 527M17 | 16MnCr5 |
Chemical composition % of steel 16MnCr5 (1.7131): EN 10084-2008
C | Si | Mn | P | S | Cr |
0.14 - 0.19 | max 0.4 | 1 - 1.3 | max 0.025 | max 0.035 | 0.8 - 1.1 |
EN 10084: 2008 Case hardening steels. Technical delivery conditions
EN 10132-2: 2000 Cold rolled narrow steel strip for heat treatment.Case hardening steels
EN 10263-3: 2001 Steel rod, bars and wire for cold heading and cold extrusion.case hardening steels
EN 10297-1: 2003 Seamless circular steel tubes Non-alloy and alloy steel tubes.
DIN 16MnCr5 1.7131 steel is widely used for a variety of applications in the used to the gearings in rotating machinery. Typical applications such as valve bodies, pumps and fittings, the high load of wheel, bolts, double-headed bolts, gears, internal combustion engine. Electric locomotives, machine tools, tractors, steel rolling equipment, boring machine, railway vehicle, and mining machinery transmission shaft on the steel ball, roller and shaft sleeve, etc.
Annealing
Slowly heated to 790-810 ℃ and allow enough times, let the steel to be thoroughly heated, Then cool slowly in the furnace. Different annealing ways will get different hardness.The 16MnCr5 will get Hardness MAX 248 HB (Brinell hardness
Quenching and temperature
Heated slowly to 788°C, Then put in salt-bath furnace keep 1191 ℃to 1204 ℃。quenching by oil get 60 to 66 HRc hardness. High temperature tempering: 650-700℃,cool in air, get hardness 22 to 30HRC. Low temperature tempering: 150-200 ℃, Cool in ari, get 61-66HRC hardness.
Hot work and cold work
DIN 16MnCr5 steel can hot worked at 205 to 538°C, 16MnCr5 can be cold worked using conventional techniques in the annealed or normalized conditions.
1 EAF: Electric Arc Furnace
2 EAF+LF+VD: Refined-smelting and vacuum degassing
3 EAF+ESR: Electro Slag Remelting
4 EAF+PESR: protective atmosphere Electro Slag Remelting
5 VIM+PESR: Vacuum induction melting
1 Hot rolling process
2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging
1 +A: Annealed (full/soft/spheroidizing)
2 +N: Normalized
3 +NT: Normalized and tempered
4 +QT: Quenched and tempered (water/oil)
1 Black Surface
2 Grounded: Bright but rough ; Not precision
3 Machining for plate: Bright and precision; Little turning scar
4 Peeled/Turned: Bright and precision; Little turning scar
5 Polished: Very Bright and precision size; Not turning scar
1 Cutting: Small pieces
2 CNC Machine: Produce as your drawing
3 Package: Bare/Nylon/Canvas/Wooden
4 Payment:T/T, L/C, O/A(request credit)
5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)